Tricot does not stay constant when construction changes. Understanding the direction of change helps during development.

Effect of knit structure

Loop length and density move results first, usually before any yarn change is made. Working figures for Tricot normally sit around 80-180 GSM in mainstream production. Note warp knit construction on the tech pack so nobody tests against an older revision.

Effect of elastane content

More elastane raises recovery but changes the value measured by warp knit construction, so retest after any blending change. Record elastane content alongside Tricot, because blends shift the measured value. A result outside 80-180 GSM usually points to process drift rather than to the fibre itself.

Tricot How It Changes with Construction and Elastane Content

Effect of finishing

Heat setting and softeners shift results, which explains differences between a hand sample and bulk. Keeping reference values for Tricot lets suppliers quote without extra sampling rounds. Ask for conditioning details together with warp knit construction, since both affect the reading.

Typical range

Working values stay around 80-180 GSM for mainstream activewear. Working figures for Tricot normally sit around 80-180 GSM in mainstream production. Note warp knit construction on the tech pack so nobody tests against an older revision.

Development advice

Change one variable at a time, then verify against warp knit construction before moving to the next sample round. Record elastane content alongside Tricot, because blends shift the measured value. A result outside 80-180 GSM usually points to process drift rather than to the fibre itself.