Tricot is verified through warp knit construction. Knowing how the method works avoids rejecting fabric that actually meets the requirement.

Method overview

warp knit construction defines sample size, conditioning and calculation, so values are comparable only within the same revision. Working figures for Tricot normally sit around 80-180 GSM in mainstream production. Note warp knit construction on the tech pack so nobody tests against an older revision.

Result interpretation

Read the value together with construction notes; 80-180 GSM is only meaningful for similar fabrics. Record elastane content alongside Tricot, because blends shift the measured value. A result outside 80-180 GSM usually points to process drift rather than to the fibre itself.

Tricot Test Methods and Acceptable Limits

Typical limits

Buyers commonly write 80-180 GSM with a stated tolerance, then verify against warp knit construction. Keeping reference values for Tricot lets suppliers quote without extra sampling rounds. Ask for conditioning details together with warp knit construction, since both affect the reading.

Sources of variation

Conditioning time, operator technique and shade all influence the result. Working figures for Tricot normally sit around 80-180 GSM in mainstream production. Note warp knit construction on the tech pack so nobody tests against an older revision.

Documentation

Record the standard revision on every report, because older versions can differ from current practice. Record elastane content alongside Tricot, because blends shift the measured value. A result outside 80-180 GSM usually points to process drift rather than to the fibre itself.