UV Degradation Solutions for Swimwear: Specification Checklist
Use this checklist to write uv degradation requirements for swimwear into a tech pack that a mill can quote against.
Targets to fix before sampling
Write UPF above 50 after 40 hours exposure into the pack. Mills quote against the number on the page, so vague language leads to variable results. Because the fabric stays wet, stretched and chemically exposed for hours, target checks are made on a worn sample rather than flat fabric alone.
Fabric construction
State structure, composition and finish together. Typical options for this build are nylon and polyester knits at 190-230 GSM with high elastane, adjusted to the performance level required. Keep AATCC 183 UPF and ISO 105-B02 light fastness named in the tech pack so every lot is measured the same way.

Seam and trim requirements
The problem shows as colour fading and strength loss after sun exposure. Construction choices either remove the cause or hide it for a few washes, so specify the method instead of the outcome. Where swimwear is worn for pool training and beach use, set tolerances around that range of movement.
Laboratory to request
Ask for AATCC 183 UPF and ISO 105-B02 light fastness on every shade and every size run, not only the approval sample. Any change to nylon and polyester knits at 190-230 GSM with high elastane requires re-testing against UPF above 50 after 40 hours exposure before bulk is released.
Acceptance criteria
Agree the limit before sampling starts. Re-testing after disagreement costs more than setting the target clearly at the beginning. Past reports from AATCC 183 UPF and ISO 105-B02 light fastness help the mill reproduce the same recipe on the next order.