Tear Strength Specification Targets for Buyers

Source:Product Wiki / Time:2026-09-16

Setting Tear Strength correctly on a tech pack prevents most later disputes. Targets belong on the page before the first fabric sample.

Where to write it

Place Tear Strength next to composition and weight so all three are quoted as one package. Working figures for Tear Strength normally sit around above 10 N typical in mainstream production. Note ISO 13937-2 trouser tear on the tech pack so nobody tests against an older revision.

Reference level

Typical activewear expectation: above 10 N typical. Record elastane content alongside Tear Strength, because blends shift the measured value. A result outside above 10 N typical usually points to process drift rather than to the fibre itself.

Tear Strength Specification Targets for Buyers

Tolerances that work

Allow a small tolerance rather than a fixed number, since normal process variation exists in every lot. Keeping reference values for Tear Strength lets suppliers quote without extra sampling rounds. Ask for conditioning details together with ISO 13937-2 trouser tear, since both affect the reading.

Verification method

Confirm with ISO 13937-2 trouser tear and keep the report against the bulk record. Working figures for Tear Strength normally sit around above 10 N typical in mainstream production. Note ISO 13937-2 trouser tear on the tech pack so nobody tests against an older revision.

Commercial note

Tightening beyond practical need raises cost without improving garment life, so set the tightest target only where it protects the customer. Record elastane content alongside Tear Strength, because blends shift the measured value. A result outside above 10 N typical usually points to process drift rather than to the fibre itself.