Durable Water Repellent (DWR) Setting It Correctly on a Tech Pack
Durable Water Repellent (DWR) should be written into the tech pack with a value, a tolerance and a method. This removes ambiguity from quotations.
Definition to agree
finish that makes water bead off. Working figures for Durable Water Repellent (DWR) normally sit around after 20 washes still grade 3+ in mainstream production. Note AATCC 22 after ISO 6330 washing on the tech pack so nobody tests against an older revision.
Target value
Open the specification at after 20 washes still grade 3+, adjusted to the end use. Record elastane content alongside Durable Water Repellent (DWR), because blends shift the measured value. A result outside after 20 washes still grade 3+ usually points to process drift rather than to the fibre itself.

Method line
Always pair the target with AATCC 22 after ISO 6330 washing so the mill and the laboratory test the same way. Keeping reference values for Durable Water Repellent (DWR) lets suppliers quote without extra sampling rounds. Ask for conditioning details together with AATCC 22 after ISO 6330 washing, since both affect the reading.
Tolerance line
State plus or minus limits to keep production realistic while protecting the requirement. Working figures for Durable Water Repellent (DWR) normally sit around after 20 washes still grade 3+ in mainstream production. Note AATCC 22 after ISO 6330 washing on the tech pack so nobody tests against an older revision.
Approval step
Approve the result on pre-production bulk rather than on development fabric only. Record elastane content alongside Durable Water Repellent (DWR), because blends shift the measured value. A result outside after 20 washes still grade 3+ usually points to process drift rather than to the fibre itself.